Order an ITO sputtering target by specifying the composition basis, material documentation and complete assembly geometry. “ITO, high purity, standard size” leaves too much unresolved: two quotations can use different percentage conventions, thickness definitions or backing-plate scopes while appearing to describe the same item.
This guide helps a laboratory turn an existing process requirement into a reviewable purchase specification. It does not prescribe a deposition recipe or promise film performance. Start with the Basis Materials ITO target page, then attach the requirements below to your inquiry.
1. Define exactly what the composition means
An oxide-weight ratio and an elemental atomic ratio are different specifications. For example, KJL explicitly identifies one commercial ITO material as In2O3/SnO2 90/10 wt.%. That label refers to the masses of the two named oxides, not to 90 atomic percent indium and 10 atomic percent tin. It is a sourced commercial example, not the assumed composition of every ITO target or every Basis configuration. [1]
When comparing a previous certificate with a new quote, retain the chemical formulas, order of components and percentage basis. If the document only says “90/10,” ask for clarification. Do not silently convert it to another convention. Converting oxide masses to elemental atom fractions requires formula masses and an explicit definition of which atoms are included in the denominator.
Distinguish a requested nominal composition from a measured lot result. Ask whether the supplier's document describes starting constituents, the finished target or a nominal product designation. If a tolerance or analytical verification is required, define it in the purchase requirement; do not infer one from the number of digits in a catalog label.
2. Separate the source target from the deposited film
A target designation does not specify the final film's resistivity, optical transmission or composition. A primary study of ultrathin RF-sputtered ITO films found changes in electrical and optical behavior with oxygen concentration under its particular deposition conditions. Its results show why process conditions belong in the discussion, not why one set of results should be guaranteed for another laboratory. [2]
Keep target acceptance and process qualification in separate parts of your specification. For the target, identify the required material and documentation. For the film, retain your substrate, thickness, deposition and post-treatment conditions, along with the measurement methods. If you require a demonstrated film result, describe the agreed test configuration rather than treating “ITO” as the acceptance criterion.
3. Keep purity, density and relative density separate
Purity describes a chemical reporting basis. Measured target density describes mass per volume for the stated measurement and specimen. Relative density compares a measured value with a specified reference density. These quantities answer different questions; none should replace the others on an RFQ.
| Reported item | Clarification to request |
|---|---|
| Nominal composition | Oxide formulas, ratio order, weight or atomic basis, and whether the value is nominal or measured |
| Purity | Reporting basis, included or excluded elements, impurity limits and whether results are lot-specific |
| Target density | Measured value, units, method and whether it represents this target, a lot sample or typical material |
| Relative density | Measured numerator and reference denominator, including the composition and conditions used for that reference |
KJL labels its listed ITO density as theoretical density. That is not a measured density certificate for a delivered Basis target. [1] When a quotation gives a percentage density, request the reference and test method before comparing it with another supplier's figure. For chemical reporting conventions, see the metal purity and COA guide.
4. Dimension the target and the complete assembly
Provide a drawing with units, revision and the surfaces that control fit. Target diameter and target thickness describe the ceramic component. Backing-plate diameter, plate thickness, bond layer and total assembly height describe additional parts of the installed stack. A correct target diameter alone does not establish that the assembly will fit.
Identify any shoulders, chamfers, recesses, mounting holes and required orientation. State whether a supplied equipment drawing controls the order or is only a reference. Mark firm interface dimensions separately from dimensions on which you would welcome a supplier recommendation. Ask the quotation to list deviations explicitly.
If replacing an existing assembly, send its identification and drawings rather than only a photograph. Specify whether the inquiry covers a bare target, a target bonded to a new plate, or review of an existing plate. Reuse and rebonding require assessment of the actual component; they are not automatic options for every order.
5. Specify equipment and bonding context
Do not assume all oxide targets require RF, or that every ITO assembly can use the same DC configuration. KJL lists ITO among conductive materials in its system's DC-power discussion. That equipment-specific example supports asking about the actual target and source configuration; it does not approve another cathode, target or power setting. [3]
Supply the cathode model, power mode, installation orientation and relevant operating history. Ask the equipment and target suppliers to confirm applicable guidance. A power-supply rating is not automatically the allowable target power. Likewise, bonding is a heat-transfer and support decision with its own constraints, not permission to increase power without review.
For joining-method comparisons, use the existing target bonding guide and bonding services overview. For structure and manufacturing questions, see how to choose a sputtering target. These references help organize the inquiry without turning the purchase order into an unverified operating procedure.
6. Copy-ready ITO RFQ checklist
Material: ITO; exact oxide or elemental designation, composition and percentage basis.
Documentation: Requested purity basis, relevant impurity limits, lot traceability, density evidence and agreed measurement methods.
Target: Diameter or shape, ceramic thickness, edge features, tolerances, units and drawing revision.
Assembly: Bare or bonded; backing-plate material and drawing, total height, bond requirement or request for recommendation.
Equipment: Cathode model, power mode, mounting orientation and relevant installation reference.
Replacement context: Previous assembly identification, known process changes and any damage requiring review.
Supply: Quantity, packaging, requested timing and inspection documents; identify unresolved requirements.
Compare the returned quotations line by line against this same checklist. Keep a missing value marked “not confirmed.” A supplier's proposed alternative should be identifiable before approval, particularly when composition basis, plate design or inspection scope changes. Resolve commercial details in the quotation instead of assuming stock, delivery time or certification from a product-family page.
Browse ceramic and compound sputtering targets, or request an ITO quotation with the drawing and specification. Confirm the offered configuration and documentation for the particular order.
Common ordering questions
Is 90/10 oxide weight the same as 90/10 elemental atomic percent?
No. The chemical species and denominator differ. Preserve the original labels and request clarification before accepting a substituted convention.
Does high relative density prove high chemical purity?
No. Request chemical evidence and density evidence separately, each with its reporting basis and sample identity.
Can a target quotation guarantee my film's transmission?
Only an explicitly agreed qualification can address a defined film result. Target composition alone does not supply the deposition conditions or measurement protocol.
Technical references
- Kurt J. Lesker: ITO In2O3/SnO2 90/10 wt.% sputtering targets. Commercial composition and theoretical-density labeling; specifications are not transferred to Basis products.
- Influence of Oxygen Concentration on the Performance of Ultra-Thin RF Magnetron Sputter Deposited Indium Tin Oxide Films as a Top Electrode for Photovoltaic Devices. Primary experimental study; results are specific to its films and process conditions.
- Kurt J. Lesker: PRO Line PVD 75 deposition platform. Equipment-specific power-supply discussion, not a universal ITO operating approval.